Product Details:
|
Raw Material: | 100% Virgin Polypropylene | Density(g/cm3): | 0.91 |
---|---|---|---|
Tensile Strength (Mpa): | 500 Min. | Melting Point(℃): | 160—170 |
Fiber Type: | Monofilament (Microfiber) | Acid &Alkali Resistance: | Strong |
Highlight: | 18mm PP Monofilament Fibre,Reinforced Concrete PP Monofilament Fibre |
500Mpa Tensile Strength Staple Filament Polypropylene Fibre Monofilament Replace Steel Net Using In Plastering
PP Monofilament Fiber Description:
Resist to shrink & crack | Increase seepage resistance |
Increase friction resistance | Increase freezing & thawing resistance |
Improve tendons protection | Replace steel net (using in plastering) |
Prevent mortar split and crackle expansion | Increase impact resistance and peeling resistance |
PP Monofilament Fiber Feature:
1. Easy to be dispersed in mortar or concrete and no agglomeration, it can guarantee the property of crack resistance effectively.
2. No need to change the proportion of mortar, just put the fibers into the mortar mixture and stir for a moment after adding water.
3. It with fine economic property: The equivalent diameter of the fiber is only φ 30um, so the ratio of diameter and surface area is high and on the basis of crack resistance, it can reduce the amount (to about 0.6kg/m 3 ).
4. Easy to plaster: As the great number of thin fibers spread into mortar evenly, the plastering is much easily and this can improve the binding strength between surface and base.
PP Monofilament Fiber Suitable Project:
A). Be suitable for the water–proof layer, floor, inner &outer wall of industrial and civil construction.
B). Increase cracking resistance on the surface of industrial workshop, warehouse and parking lot.
C). Increase cracking & seepage resistance of the ground in natatorium, swimming pool, pond and ditch.
D). Be suitable for any mortar projects and fine aggregate concrete projects .
PP Monofilament Fiber Applying Instruction:
A). Compound Amount. To resist the common cracks on surfaces, 0.6kg/m3 fibers to cement paint is enough, and for reinforced application 0.9-1kg/m3 is enough.
B). Stirring requirement. The proportion of cement, sand and aggregate is no need to be changed. Put cement, aggregate, additive and fiber together, then stir after adding enough water (Do not stir without water!) and time for stirring can be prolonged for 2~3 minutes in order to make the compound mix completely.
Contact Person: Linda Qiang
Tel: 0086-13856999452
Fax: 86-551-63517768